FAIZEAL · CUSTOM MAGNETIC COMPONENTS · OEM AND ODM
A very long travel begins as a very precise magnetic surface. This is a customer-specific NdFeB magnet track module: hundreds of plated magnet tiles bonded to a machined steel yoke, phased so that pole pitch stays continuous across every joint.
Flat permanent-magnet linear motor secondary · Segmented sintered NdFeB array on a black-coated steel back yoke · Counterbored mounting rails with dowel location · Per-tile magnetisation reference marks · Module-to-module pole-phase continuity verified in-house by FAIZEAL
This assembly is the stationary magnet track, or secondary, of a flat permanent-magnet synchronous linear motor. It is not a complete motor. The moving forcer, its three-phase windings, the bearing system, the encoder and the drive are supplied by the machine builder; what FAIZEAL supplies is the magnetic surface that sets the performance ceiling for all of them.
The photograph shows one module of a very long track. A black-coated machined steel yoke carries a regular array of silver-plated rectangular magnet tiles, bounded on both long edges by a row of counterbored mounting holes and smaller dowel or pilot holes. Each tile carries a short red reference line. The module is designed to be bolted to a machine base and butted end to end with its neighbours until the required stroke is reached.
Very large is the point of this product. A track several metres long cannot be made as one monolithic magnet, cannot be plated in one bath, cannot be magnetised in one pulse, and cannot be shipped or lifted as one magnetised assembly. It has to be engineered as a set of modules whose individual precision accumulates into one continuous magnetic field.
That accumulation is where projects succeed or fail. A local flatness error, a tile with reversed polarity, a bond line that is a little too thick, or a joint gap that shifts the pole phase by a fraction of a pole pitch will all show up later as thrust ripple, velocity ripple, or a position error that the controller cannot tune out. Every one of those is decided on this plate.
FAIZEAL designs and builds these tracks as custom components. Pole pitch, tile geometry, magnet grade, coating, yoke material, mounting pattern, module length, joint strategy and inspection plan are all set against the customer's forcer and motion profile, then verified on the finished assembly before it leaves the factory.
The image is worth reading closely, because almost every visible feature is a functional decision rather than a cosmetic finish.
What the photograph shows | What it means for the design |
Black, glossy machined steel plate with chamfered ends and a bright silver side edge | The structural yoke and, in conventional topologies, the magnetic back iron. The machined side edge is the alignment datum used when the module is set on the machine base |
A row of large counterbored silver holes along both long edges | Through-bolt mounting with the fastener head recessed below the working face, so the forcer never passes over a protruding screw |
Smaller holes spaced between the counterbores | Dowel or pilot locations that fix the module's angular and lateral position without relying on bolt clearance |
A regular grid of rectangular silver tiles with bright chamfered edges | Sintered NdFeB magnet segments. Several tiles laid side by side across the width form one pole bar; the chamfers protect brittle corners and keep the bond line uniform |
Thin, even dark lines between every tile | Controlled inter-tile gaps filled with non-magnetic potting, leaving no exposed steel, no chip trap and no crevice for coolant or corrosion to creep beneath the plating |
A short red line on each tile | A magnetisation-direction reference applied during tile sorting. It is a handling and traceability mark, not proof of polarity; the north-south sequence is verified by a Hall scan of the finished face |
Champagne-to-silver metallic tile faces | Ni-Cu-Ni triple-layer plating, typically 20 to 35 µm. Epoxy, parylene or a sealed metal cover is specified where the environment demands it |
Long, narrow aspect ratio with many tile columns along the length | A single module of a multi-module track. Stroke is extended by joining identical modules, not by scaling one magnet up |
Notice what is not in the photograph. There are no coils, no cables, no encoder, no bearing rails and no cover plate over the magnets. That is deliberate. We supply the magnetic half of the motor and leave the working face accessible, so the machine builder can set and measure the air gap directly.
The first limit is material. Sintered NdFeB is pressed in a magnetic field and sintered as a discrete block. Press size, plating bath size, grinding table size and magnetising coil bore all cap the size of a single magnet. A pole bar a metre wide cannot be produced in one piece, so each pole is assembled from several tiles laid side by side across the width.
The second limit is force. A magnetised track several metres long pulls on every steel tool, fixture, gantry and fastener near it, while adjacent tiles push against one another as they are being positioned. Assembly has to be done with non-magnetic fixtures, progressive placement and controlled hold-down, or tiles chip, flip, or land out of position. This is a handling problem before it is a magnetic one.
The third limit is geometry. The working air gap between the forcer and the magnet face is typically on the order of 0.5 to 1.5 mm, so flatness and straightness over metres matter more than absolute size. Steel expands by roughly 12 µm per metre per kelvin; a ten-degree temperature gradient along a three-metre machine moves the ends by about 0.36 mm, which is a large fraction of the air gap.
FAIZEAL holds straightness to 0.02 mm per 1000 mm module and 0.05 mm per metre over an assembled track, then designs the mounting so that one module is the fixed datum and the rest can float in a controlled direction. Thermal growth is allowed to happen without dragging the pole pattern out of phase.
The fourth limit is time. Hundreds of tiles on one plate means hundreds of bond lines. Adhesive open time, dispensing volume, bond-line thickness and cure pressure have to stay constant from the first tile to the last, or the working face ends up subtly stepped. A 0.05 to 0.20 mm controlled bond line, held by a pressure fixture through cure, is what keeps the array coplanar.
The fifth limit is logistics. A magnetised assembly of this size is a strong magnetic source; it cannot be shipped loose, cannot be machined afterwards, and cannot be reworked on site without disturbing its field. The track is therefore divided into modules that can be handled, packed in non-magnetic protection, and bolted down in sequence. Segmentation is a manufacturing strategy, not a compromise.
In a three-phase linear motor the pole pitch sets the electrical wavelength. Standard pitches run from 12 mm to 60 mm, with custom values from 5 mm to 120 mm, and the forcer's coil geometry is matched to that pitch. Get the pitch right and thrust is proportional to current; get it wrong and no amount of drive tuning recovers the lost force.
Standard module lengths are 96, 144, 192, 240, 288 and 384 mm, with custom segments up to 1000 mm. Modules are joined end to end to build tracks from 100 mm to more than 10 metres. The upper limit on stroke is set by cable management and the machine base, not by the magnet technology.
The joint is the hard part. It is not merely a mechanical seam; it is a magnetic seam. If the gap between two modules makes the pole phase drift by even a small fraction of a pole pitch, the forcer sees a once-per-module disturbance. At low speed that becomes a velocity ripple; on a scanning axis it becomes a visible band in the image or in the machined surface.
FAIZEAL treats the joint as a controlled feature. Module ends are machined square to the pole pattern, the pole sequence is specified to continue across the boundary, and a setting gauge or dowel-and-slot arrangement fixes the gap during installation. One fixed datum and floating holes then absorb thermal growth without opening the joint.
The two ends of a finite track have their own signature. Because the magnetic circuit stops there, the forcer sees a changing reluctance as it enters and leaves, which produces end-effect force ripple. Where the motion profile demands it, the end tiles, the pole arc or the forcer's commutation are adjusted to compensate. This is reviewed at the design stage with the machine builder, not discovered during commissioning.
Every module is serialised, and the joint gap and pole-phase record are kept with the batch. A replacement module supplied two years later can be matched to the original field rather than merely to the original drawing.
A flat permanent-magnet linear motor is a rotary servo motor unrolled into a straight line. The forcer's three-phase windings are commutated electronically to create a travelling field that couples to the stationary north-south sequence of the track. Thrust is directly proportional to current, with no leadscrew, belt, rack or gearbox in between, so there is no backlash, no mechanical wear and no transmission loss to compensate for.
Two topologies are common. In a conventional track, alternating north and south tiles sit on a steel back iron that closes the flux path. It suits an iron-core forcer, which concentrates flux in laminated poles and delivers roughly two to four times the continuous thrust of an equivalent ironless unit, at the cost of a constant attraction force and a periodic cogging force of roughly one to three percent of rated thrust.
The alternative is a Halbach track, where the magnetisation vector rotates from segment to segment so that flux adds on the working face and cancels on the back. Air-gap flux density rises by 30 to 50 percent, the back iron can be thinned or removed, stray field behind the track falls sharply, and the near-sinusoidal field cuts cogging by 60 to 80 percent. It is the preferred route for ironless forcers and ultra-precision stages.
The gain is a design variable, not a fixed bonus. For three segments per pole pair the field gain factor is about 1.5, for four about 1.707, and a continuously rotating magnetisation approaches 2. In practice three to six segments per pole period balance field gain against assembly complexity, and the choice is made together with the forcer designer.
The black plate in the photograph is the structural yoke of the delivered module. Depending on the motor topology it may also be the magnetic return path, or the array above it may be a Halbach stack that needs little or no back iron. FAIZEAL does not assume which one applies; the yoke material, thickness and magnetic role are set against the customer's forcer specification.
Whatever the topology, the air gap is the design. Air-gap flux density falls on roughly a squared trend as the gap grows, so a local step of a tenth of a millimetre from a proud tile or a bowed yoke changes thrust at that point. This is why tile coplanarity, yoke flatness and mounting are treated as magnetic parameters rather than as finishing operations.
The tiles are sintered NdFeB. Standard grades N42 to N52 give remanence of roughly 1.05 to 1.45 T and maximum energy products of 240 to 474 kJ/m³. Where the track runs hot, high-coercivity variants N42SH, N40UH, N38EH and N33AH extend operation from 80 °C up to around 200 °C or higher. SmCo is available where temperature stability and corrosion resistance outweigh raw flux.
Temperature is a design input, not an afterthought. The remanence of NdFeB falls by about 0.11 percent per kelvin, and intrinsic coercivity falls by roughly 0.55 to 0.65 percent per kelvin. Coil heat conducted into the track therefore reduces available flux and, more seriously, moves the operating point toward the knee of the demagnetisation curve. FAIZEAL sizes the grade with at least a 1.3 times demagnetisation margin at the worst-case operating point.
The champagne-silver faces in the photograph are Ni-Cu-Ni triple-layer plating, typically 20 to 35 µm. For chemical, marine or high-humidity service an epoxy coating is used; for vacuum, semiconductor and medical environments parylene or a sealed stainless or aluminium cover is specified. Plating is applied to each tile before bonding, because spraying a finished assembly would bridge the insulating gaps between tiles and trap corrosive residue.
Every tile carries a short red line. It is a magnetisation-direction reference applied during tile sorting, so that each piece is placed with its vector pointing the right way. A reversed tile looks exactly like a correct one from the outside; the mark is a handling aid and a traceability record, not proof of polarity. The actual north-south sequence is verified by a Hall scan of the finished face.
The bright chamfer on each tile edge is functional. Sintered NdFeB is brittle, and a sharp corner chips during placement and creates a local flux spike. Chamfers also let the adhesive form a uniform meniscus rather than a void. The thin gaps between tiles are then filled with a non-magnetic potting compound, leaving a continuous, cleanable working face with no exposed steel and no place for swarf or coolant to collect.
Cogging is the periodic pull between the track's magnets and the iron teeth of an iron-core forcer. It is typically one to three percent of rated thrust, and because it repeats with position it feeds directly into the velocity loop. On a scanning axis it limits settling time and can leave visible banding; on a machine-tool axis it can mark the surface finish.
Three levers reduce it. Skewing the magnets by five to ten degrees averages the tooth interaction and can cut cogging by 60 to 80 percent at a cost of one to three percent in back-EMF. Optimising the pole arc makes the field more sinusoidal. Fractional-slot coil layouts reduce the harmonic content that the controller would otherwise have to cancel.
A tiled track adds its own, finer signature. If the gaps between tiles vary, or if one tile sits slightly high, the forcer sees a small dip once per tile pitch. On a very large plate with hundreds of tiles, that is hundreds of opportunities for a periodic error, which is why gap width, bond-line thickness and coplanarity are controlled as a single process rather than inspected tile by tile after the fact.
Module joints add a second, coarser period, and the two ends of the track add a third. FAIZEAL controls pole-arc coefficient to within one degree and magnetisation-direction deviation to within one degree, then measures the assembled field rather than inferring it from the drawing. The result is a force ripple budget the machine builder can design against instead of discovering during commissioning.
An ironless forcer removes the tooth interaction altogether and is the right answer when speed stability and sub-micron settling dominate. It gives up thrust density, so the track has to be sized accordingly. FAIZEAL will recommend it when the motion profile calls for it, even though it usually means a larger magnet surface.
The forcer is the heat source, but the track is the surface it sits above. Continuous thrust is a thermal limit, and peak thrust, typically two to four times continuous, is only available for the short intervals the winding can absorb. FAIZEAL needs the duty cycle, not just the peak force, to select a grade and a coating that will hold their properties for the life of the machine.
At high speed the track sees a high-frequency field. Sintered NdFeB is electrically conductive, so a solid tile develops internal eddy currents.
Where the electrical frequency is high, FAIZEAL can build each pole from laminated slices 0.20 to 0.50 mm thick with a 10 to 25 µm insulating layer between them. Because loss scales with the cube of slice thickness, this cuts magnet eddy-current loss by 60 to 90 percent and reduces magnet temperature rise by 30 to 50 percent.
Semiconductor wafer and reticle stages, with very high acceleration and velocity, commonly call for laminations of 0.20 mm or less. Insulation coverage must include every edge, because one pinhole reconnects the slices and creates a local hot path. Insulation resistance between adjacent slices is checked at greater than 10 MΩ at 100 V as part of the standard flow.
Cleanroom, vacuum and dry-room service change the specification more than the magnetic design does. Outgassing, particle shedding, corrosion from cleaning agents, and metal ions near the process all have to be excluded. Sealed covers, parylene, edge potting, low-outgassing adhesives and documented cleaning are specified with the customer, and the finished face is left smooth and crevice-free so it can be wiped down.
Finally, there is the field itself. A track of this size is a strong magnetic source. FAIZEAL supplies handling instructions, non-magnetic packing, and a defined safe-working envelope for installation, and advises on shielding and on the stand-off distance to encoders, sensors and ferrous machine elements. This is part of the delivery, not an afterthought.
The process order is fixed, because magnetised parts cannot be machined. Everything that cuts, drills, grinds or coats the yoke and the tiles happens first. Magnetisation comes last, and after it the assembly is only measured, cleaned, protected and packed. Reworking a magnetised track would disturb the field and draw ferrous debris onto the working face.
Each magnet batch is checked for Br, Hcj and BHmax on a vibrating-sample magnetometer or Helmholtz coil, then dimensionally and visually inspected for cracks, chips and plating defects. Yoke flatness, straightness, counterbore geometry and dowel position are verified by CMM before any magnet is bonded. Mating surfaces are held to Ra 0.4 to 0.8 µm.
Tiles are sorted by polarity and orientation, then placed with a non-magnetic progressive fixture. A structural adhesive is dispensed to a controlled 0.05 to 0.20 mm bond line and held under pressure through cure. Room-temperature anaerobic systems such as Loctite 326 with activator 7448 suit assemblies that must not be baked; two-component high-temperature epoxies are used where the service temperature demands them.
Magnetisation is done on a fixture designed with finite-element simulation of the coil, locating mandrel and magnetic shielding. NdFeB needs a pulse field of two to three times its intrinsic coercivity Hcj to saturate fully, and the coil is matched by grade so that no tile is left looking magnetised but actually weak. Pole-arc coefficient is held within one degree; skewed, Halbach and custom field profiles are available.
Every finished module is then scanned by a flux mapper at a defined air-gap plane. The check catches a reversed tile, a weak tile, a wrong pole count, a pole-arc deviation and a non-uniform gap, and flux uniformity is held within three percent. This is the single most important inspection on the part, because the defects it finds are invisible in the photograph.
Final checks cover overall dimensions, flatness, straightness, tile coplanarity and coating thickness; bonded samples are pull-tested to greater than 20 MPa shear; and the serialised field fingerprint, material certificates and inspection report travel with the batch. The first article becomes the reference against which every later module is compared.
The following are capability ranges rather than a fixed product. The values that appear on the final drawing are the ones that the customer's forcer, air gap, duty cycle and machine base require.
Parameter | What FAIZEAL can build |
Motor topology | Conventional north-south array on steel back iron, or Halbach array; matched to iron-core or ironless forcer |
Magnet material and grade | Sintered NdFeB N42 to N52; high-temperature N42SH, N40UH, N38EH, N33AH; SmCo on request |
Pole pitch | 12 to 60 mm standard; 5 to 120 mm custom |
Segments per pole period | Conventional single-pole tiles; Halbach arrays with 3, 4 or 6 segments per pole period |
Module length | 96, 144, 192, 240, 288 and 384 mm standard; up to 1000 mm custom |
Total track length | 100 mm to more than 10 m by joining modules |
Straightness | 0.02 mm per 1000 mm module; 0.05 mm per metre over an assembled track |
Pole arc and direction | Pole-arc coefficient within 1 degree; magnetisation-direction deviation within 1 degree |
Flux uniformity | Within 3 percent across the working face |
Bond line | 0.05 to 0.20 mm, pressure-held through cure |
Coating and sealing | Ni-Cu-Ni 20 to 35 µm; epoxy, parylene, black epoxy; stainless or aluminium cover; edge potting |
Laminated option | Slices 0.20 to 0.50 mm with 10 to 25 µm insulation; 0.20 mm or less for semiconductor stages |
Inspection and records | CMM, flux mapping, pull test, coating thickness, salt spray, serialised field fingerprint and reports |
Semiconductor wafer and reticle stages. Lithography, inspection and metrology axes using ironless forcers with finely pitched or Halbach tracks, sub-micron settling, cleanroom-class construction, and laminated tiles where acceleration is extreme.
Flat-panel display manufacturing. LCD, OLED and micro-LED inspection, repair and laser annealing over one to five metre strokes, where speed stability below 0.1 percent and a ripple-free scan decide image quality.
Precision machine tools and laser processing. CNC axes, laser and waterjet cutting heads, and grinding stages using iron-core forcers for high continuous thrust, with joint and end effects budgeted so the surface finish does not show the track seams.
High-speed pick and place. Surface-mount placement, component insertion and packaging lines, where acceleration above 10 g and sub-millisecond response set the cycle time.
Metrology, automated optical inspection and scanning. Vision systems, X-ray detectors, laser scanners and coordinate measurement, where a smooth low-speed velocity profile is worth more than peak force.
Solar, battery and large-format automation. Cell printing, electrode coating and inspection, module assembly and large gantry axes in dry rooms, where multi-metre tracks and modular replacement keep the line running.
Planar and multi-axis platforms. Two-dimensional positioning stages, large-format printing and gantry systems where several tracks must share one flatness datum and one pole-phase reference.
FAIZEAL is a magnet engineering and manufacturing company, not a trading company. Precision machining, magnetising fixture design, magnetisation, bonding, flux mapping and inspection are carried out in-house. Magnet tracks, Halbach arrays and magnetic semi-assemblies are core products rather than sidelines.
On a part like this the pole pitch, the tile gaps, the joint strategy, the yoke flatness and the thermal design are one coupled system, and they have to be engineered by the team that builds them. We have supplied custom magnetic assemblies to robotics, new-energy, semiconductor and industrial customers in more than 30 countries since 2017.
Finite-element-based magnetic and structural assessment is part of the design review rather than a paid extra. Small-batch, multi-variety production is normal for us, because large custom tracks are what we build. We also say when a customer would be better served by a standard catalogue track, or by a different motor topology altogether.
To start, send us the forcer type with its air-gap and field specification, the pole pitch, the continuous and peak thrust, the speed and acceleration, the required stroke and preferred module division, the machine base material and mounting pattern, the temperature range and duty cycle, the environment and cleanliness class, any coating or sealing requirements, and the target quantity.
Our engineers will return a pole-count and magnetic-circuit proposal, an air-gap and flatness budget, a joint and thermal-growth strategy, material and coating recommendations, an inspection plan, and a quotation. Prototypes are available with fast sample turnaround, and production scales on the same tooling, magnetising fixture and inspection plan.
The field fingerprint recorded on the first module becomes the reference for every subsequent batch, so a replacement supplied years later still matches the machine it goes into.
Give us the stroke, the forcer and the duty cycle. We will engineer the field. |
FAIZEAL · fzmag.com · Custom large-format linear motor magnet tracks and magnetic assemblies · sales@fzmag.com
Right-angle transmission, parallel transmission, wall-climbing robot
Right-angle transmission, parallel transmission, wall-climbing robot